Nickel Alloy C2000, 2.4675
| Alloy (UNS) | Ni | Cr | Mo | W | Cu | Fe | Carbon |
|---|---|---|---|---|---|---|---|
| C2000® (N06200) | Bal | 22.00-24.00 | 15.00-17.00 | – | 1.30-1.90 | 3.00 max. | 0.010max. |
| Heat Treatment of Finished Parts | |||||
|---|---|---|---|---|---|
| Condition as supplied by Alloy Wire | Type | Temperature | Time (Hr) | Cooling | |
| °C | °F | ||||
| Annealed or Spring Temper | Stress Relieve | 400 – 450 | 750 – 840 | 2 | Air |
| Properties | ||||
|---|---|---|---|---|
| Condition | Approx. tensile strength | Approx. operating temperature | ||
| N/mm² | ksi | °C | °F | |
| Annealed | 700 – 1000 | 102 – 145 | -200 to +400 | -330 to +750 |
| Spring Temper | 1300 – 1600 | 189 – 232 | -200 to +400 | -330 to +750 |
| Melting Point | 1399°C | 2550°F |
| Density | 8.5 g/cm³ | 0.307 lb/in³ |
| Coefficient of Expansion | 12.4 μm/m °C (20 – 100°C) | 6.9 x 10-6 in/in °F (70 – 212°F) |
| Modulus of Rigidity | 79 kN/mm² | 11458 ksi |
| Modulus of Elasticity | 206 kN/mm² | 29878 ksi |
| STANDARD | WERKSTOFF NR. | UNS | AWS |
|---|---|---|---|
| Hastelloy C2000 | 2.4675 | N06200 | AWS 055 |