Mechanical Properties of Hastelloy C22 Round Bar
| Grade | Minimum Tensile Strength | Minimum 0.2% Offset Yield Strength | Minimum Elongation (within 50mm) | Melting Point |
|---|---|---|---|---|
| Hastelloy C22 | 100,000 psi / 690 MPa | 45,000 psi / 310 MPa | 45% | 1399 °C (2550 °F) |
Hastelloy Alloy C22 Bar Chemical Composition
| Grade | C | Cr | Mo | Si | V | Fe | Ni |
| Hastelloy C22 | 0.010 max | 20 – 22.5 | 12.5 – 14.5 | 0.08 max | 0.35 max | 2 – 6 | Bal |